MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASTM A178 C 0.2C Silicon-Killed Steel Tubes for Boilers and Heat Exchangers (STB 410)
Categories: Metal; Ferrous Metal; ASTM Steel

Material Notes:

Creep and rupture data provided by NIMS

Key Words: DIN 17175 st 45.8; UNS K03503; BS 3059-P2 440; JIS G3461 STB 410
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 180 MPa
Elongation at Break 35 %
Rupture Strength 67.0 - 69.0 MPa
@Temperature 500 °C,
Time 3.60e+8 sec
 67.0 - 102 MPa
@Temperature 475 °C,
Time 3.60e+8 sec
 83.0 - 140 MPa
@Temperature 450 °C,
Time 3.60e+8 sec
 109 - 176 MPa
@Temperature 425 °C,
Time 3.60e+8 sec
 147 - 231 MPa
@Temperature 400 °C,
Time 3.60e+8 sec
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.060 - 0.18 %
Iron, Fe 99.12 - 99.67 %
Manganese, Mn 0.27 - 0.63 %
Phosphorus, P <= 0.035 %
Sulfur, S <= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A572 Steel, grade 50
AISI 1018 Steel, cold drawn
ASTM A213 T22 2.25Cr-1Mo STEEL FOR BOILER AND HEAT EXCHANGER SEAMLESS TUBES (STBA 24)
AISI 1095 Steel, as rolled
ASTM A36 Steel, bar

NIMS001 / 77518

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.