Windform TPU is a durable Thermoplastic Polyurethane, distinguishing for its unique softness and elasticity witnessed by an elongaton at break >400%. Windform TPU is designed for highly professional 3D printed parts requiring rubber-like features, high tensile strength and shock absorption. Parts realized in TPU ensures longevity and durability even under prolonged and intensive use. Applications: - Superior Softness and elasticity for durable functional parts and prototypes
- Athletic footwear and apparel
- Fashion ART & Design objects with complex geometries and soft touch
- Parts requiring highest flexibility together with shock absorption and traction resistance
- Automotive car interior components, air filter frames and details requiring softness and resistance
- Robotics components, flexible and adaptable to move and work in complex environments and accomplishing unique tasks
- Soft-touch functional prototype simulation
- Hoses, gaskets
Information provided by CRP Technology. |
About CRP Technology CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |