Product Description: Injection Molding; Characteristics: High fluidity, High impact strength Availability: Asia Pacific; Europe; North America Features: High Flow; High Impact Resistance; Impact Copolymer Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520© 3.1a RoHS Compliance: RoHS Compliant UL File Number: E162823 Processing Method: Injection MoldingInformation provided by Formosa Chemicals & Fiber Corporation |