MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CHT SE2005 Silicone elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a 2-component, silicone elastomer system specially designed for electronic potting and encapsulation applications. It offers good protection against chemicals, environmental contamination, mechanical shock, vibration and impact damage. It can be employed in areas where low flammability is a prerequisite. The cured elastomer can be repaired. The component parts have relatively low viscosities and are readily mixed either by hand or machine

Key Features

  • Low viscosity
  • Deep section cure
  • Excellent dielectric properties
  • Protects against shock and vibration
Application: Protects against shock/vibration.

Cured Product: 7 days at 23+/-2°C and 50+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³B; BS ISO 2781
 1.20 g/cc0.0434 lb/in³Cured Product; BS ISO 2781
 1.21 g/cc0.0437 lb/in³A; BS ISO 2781
Brookfield Viscosity 300 cP300 cPB
 9000 cP9000 cPMixed
 9000 cP9000 cPA
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240-95
Tensile Strength 1.08 MPa157 psiISO 37
Elongation at Break 180 %180 %ISO 37
Tear Strength 2.10 kN/m12.0 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+14 ohm-cm3.00e+14 ohm-cmASTM D-257
Dielectric Constant 3.43.4ASTM D-150
Dielectric Strength >= 18.0 kV/mm>= 457 kV/inASTM D-149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 220 °C428 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourDe-mould Time / Full Cure
Pot Life 60.0 min60.0 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
AppearanceCondensation
ColorWhite
Mix Ratio100:1By Weight
RheologyLiquid
Volume Coefficient of Thermal Expansion762 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL060 / 314543

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.