Medium reinforcing low-structure carbon black with medium dispersion. Provides higher die swell, high resilience at a relatively high hardness. High loading capacity. Tire body and tube compounds. Molded products, profile-extruded products. One-plied roofing. Insulation cable rubber.Information provided by Ganpati Exim PVT. LTD. |