Ultramid T KR 4355 G7 BK00564 is a 35% glass fiber reinforced injection molding PA6/6T grade featuring high toughness, stiffness, and strength, low water absorption, and high melting point (295 C). After the material has been conditioned, its mechanical properties remain stable up to 60 C. This grade is available in black.Information provided by BASF. |