MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
CHT AS1420 1-part, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a heat cured, non-corrosive, neutral cure, 1-part, silicone adhesive sealant. It is one in a range of Addition cure products which are solvent free. It exhibits primerless adhesion to many substrates when cured at temperatures above 100°C. It cures to form a very tough resilient silicone elastomer. This product will not corrode copper or its alloys and is suitable for use with electronic components.

Key Features

  • Fast heat cure
  • Excellent thermal conductivity
  • Non corrosive
  • Tough protective rubber
Application: Electronics

Cured Product: After 1 hour at 150°C

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.06 g/ccBS ISO 2781
Brookfield Viscosity 43000 cPMixed
Linear Mold Shrinkage 0.020 cm/cm
Storage Temperature -5.00 - 15.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67ASTM D2240-95
Tensile Strength 450 psiISO 37
Elongation at Break 70 %ISO 37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.70e+15 ohm-cmASTM D-257
Dielectric Constant 6.0ASTM D-150
Dielectric Strength 571 V/milASTM D-149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 187 µm/m-°C
Thermal Conductivity 1.38 W/m-K
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 150 °C
 2.00 hour
@Temperature 100 °C
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorGrey
Cure typeAddition Heat Cure
RheologyFlowable
Self BondingYes
Volume Coefficient of Thermal Expansion562 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL004 / 314487

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.