ATECH is a series of sheets based on ABS which is a raw material with very high impact-strength. ABS also has impressive thermal qualities and is easy to thermoform and fabricate. The ATECH 3100 is a super high impact matte ABS which remains matte after thermoforming. Also Available In: ATECH 3103 has extra UV stabilizers added to improve weather resistance; ATECH 3110 with the matte surface on both sides; Dual coloring to optimize to specific needs Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met. Benefits: Supermatt surface finish after thermoforming; Easy to thermoform; High impact strength; Good thermal qualities Application: Suitable for demanding automotive parts which are exposed to secondary UV light, and other tough industrial applications where a supermatt finish is required. Information provided by Arla Plast. |