MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin EM7301F Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ EM7301F resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits high heat resistance, good flow and polyurethane foam adhesion along with creep resistance, dimensional stability, and hydrolytic stability. NORYL EM7301F resin is an excellent candidate for automotive interior applications such as audio speaker components. This material is available only in black.

Features: Hydrolytic Stability,Good Stiffness

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 18 cP
@Load 2.16 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
Tensile Modulus 3700 MPa1 mm/min; ISO 527
Flexural Strength 90.0 MPabreak, 2mm/min; ISO 178
Flexural Modulus 3500 MPa2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1U
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 19.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 19.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.230 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 115 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 125 °CRate B/50; ISO 306
 130 °CRate B/120; ISO 306
 135 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 260 - 280 °C
Zone 2 260 - 280 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82274 / 290221

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.