MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemours Teflon™ FEP 9495 Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Fluorinated Ethylene Propylene (FEP), Molded/Extruded

Material Notes: Teflon™ FEP 9495 is a melt-processible fluoroplastic resin available in pellet form. It is a copolymer of tetrafluoroethylene and hexafluoropropylene, without additives, that meets the requirements of ASTM D 2116 Type II. With a relatively high melt flow rate and excellent electrical properties, Teflon™ FEP 9495 has been specifically designed for high-speed extrusion of thin coatings on small-gauge wires for twisted-pair constructions. Applications for Teflon™ FEP 9495 include small diameter, thin wall wire and cable insulation; industrial film; and intricate or thin wall parts made by injection molding.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D792
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 372 °C
30 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D2116
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength 20.0 MPa2900 psiASTM D638
Elongation, Ultimate 300 %300 %ASTM D638
Flexural Modulus 0.520 GPa75.4 ksiASTM D790
Flex Crack Resistance 7000
@Thickness 0.203 mm
7000
@Thickness 0.00800 in
Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBNBASTM D256
Coefficient of Friction 0.080 - 0.300.080 - 0.30ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant  2.03
@Frequency 1000 Hz
2.03
@Frequency 1000 Hz
ASTM D150
 2.03
@Frequency 1e+9 Hz
2.03
@Frequency 1e+9 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.250 mm
2030 kV/in
@Thickness 0.00984 in
ASTM D149
Dissipation Factor  0.00040
@Frequency 1e+9 Hz
0.00040
@Frequency 1e+9 Hz
ASTM D150
 0.00060
@Frequency 1000 Hz
0.00060
@Frequency 1000 Hz
ASTM D150
Arc Resistance 300 sec300 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FASTM D4591
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)200Chemours Method. 372°C
Detergent Resistance (hours)480On grit blasted aluminum.
 600On aluminum
 744
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceExcellent
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8790 / 268716

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.