MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX934 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 934 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits improved processability and excellent heat aging performance. NORYL GTX934 resin was designed for high heat automotive under-the-hood applications.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Moisture Absorption 0.0700 %0.0700 %Injection Molding
 1.21 %1.21 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.5 %3.5 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 280 °C
13 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm0.016 - 0.020 in/inSABIC method
 0.014 - 0.017 cm/cm
@Thickness 3.20 mm
0.014 - 0.017 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm
@Thickness 3.20 mm
0.011 - 0.014 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 280 °C
13 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiH358/30; ISO 2039-1
Tensile Strength at Break 55.0 MPa7980 psi50 mm/min; ASTM D638
 55.0 MPa7980 psi50 mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ISO 527
Elongation at Break 25 %25 %50 mm/min; ISO 527
 60 %60 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527
 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa334 ksi50 mm/min; ASTM D638
 2.40 GPa348 ksi1 mm/min; ISO 527
Flexural Strength 90.0 MPa13100 psiyield, 2 mm/min; ISO 178
 95.0 MPa13800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
 2.35 GPa341 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 220 J162 ft-lbASTM D256
 100 J
@Temperature -30.0 °C
73.8 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 J44.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  70.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 190 °C
@Thickness 3.20 mm
374 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 200 °C392 °FRate B/50; ISO 306
 205 °C401 °FRate B/50; ASTM D1525
 205 °C401 °FRate B/120; ISO 306
 250 °C482 °FRate A/50; ISO 306
UL RTI, Electrical 100 °C212 °FUL 746B
UL RTI, Mechanical with Impact 100 °C212 °FUL 746B
UL RTI, Mechanical without Impact 85.0 °C185 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Glow Wire Ignition Temperature  725 °C
@Thickness 0.750 mm
1340 °F
@Thickness 0.0295 in
IEC 60695-2-13
 725 °C
@Thickness 1.00 mm
1340 °F
@Thickness 0.0394 in
IEC 60695-2-13
 725 °C
@Thickness 1.50 mm
1340 °F
@Thickness 0.0591 in
IEC 60695-2-13
 725 °C
@Thickness 2.50 mm
1340 °F
@Thickness 0.0984 in
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
IEC 60695-2-12
 700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
IEC 60695-2-12
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-12
 700 °C
@Thickness 2.50 mm
1290 °F
@Thickness 0.0984 in
IEC 60695-2-12
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 310 °C536 - 590 °F
Zone 2 280 - 300 °C536 - 572 °F
Zone 3 290 - 320 °C554 - 608 °F
Melt Temperature 290 - 320 °C554 - 608 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82172 / 290119

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.