D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm to 1.1 mm. D 263® T eco borosilicate glass is available in standard stock size sheets or can be custom cut into round or square shapes. D 263® T eco thin glass is used as a substrate glass for coatings or replacement for plastic for applications in the automotive and electronics industries D 263® T eco is manufactured without adding arsenic and antimony as refining agents. It has been used in touch panel displays, optocaps for diode lasers, and other optical applications.Information provided by SCHOTT North America. |