MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem Lowinox™ CPL Stabilizer
Categories: Other Engineering Material

Material Notes: Product Description: Lowinox™ CPL stabilizer is a highly effective polymeric, non-discoloring phenolic antioxidant.

CAS No: 6861-51-5

EINECS No: 271-867-22

Application: Lowinox™ CPL stabilizer is an excellent non-discoloring, non-staining antioxidant, processing high activity and low volatility. Lowinox™ CPL stabilizer is highly recommended for the protection of isoprene and butadiene-based polymers. Lowinox™ CPL stabilizer is also recommended for the stabilization of natural rubber and latex, SBR and caboxylated SBR lattices, ABS, ASA, MBS, SBS, SIS CR, NBR, BR and for tackifiers, adhesives and sealants. Lowinox™ CPL stabilizer is highly resistant to extraction by washing and boiling making it especially suitable for use in rubber threads and latex for carpet backing and foams. Lowinox™ CPL stabilizer can be prepared as an aqueous dispersion for easier handling and addition to water-based systems.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccsolidified melt
Bulk Density 0.360 g/ccpowder
 0.600 g/ccpellet
Molecular Weight 600 - 700 g/mol
 
Thermal PropertiesOriginal ValueComments
Softening Point >= 105 °C
 
Descriptive Properties
AppearanceCream colored or amber powder or pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH502 / 315420

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.