MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC PC1000 PC  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.

This data was supplied by SABIC-IP for the Americas region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D 792
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 0.35 %
@Temperature 23.0 °C
ASTM D 570
Water Absorption at Saturation 0.35 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmon tensile bar; SABIC Method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D 785
 120ISO 2039-2
Tensile Strength, Yield 63.0 MPaType I, 50 mm/min; ASTM D 638
 63.0 MPa50 mm/min; ISO 527
Elongation at Break >= 70 %Type I, 50 mm/min; ASTM D 638
 >= 70 %50 mm/min; ISO 527
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D 638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa50 mm/min; ASTM D 638
 2350 MPa1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
 90.0 MPa2 mm/min; ISO 178
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D 790
 2300 MPa2 mm/min; ISO 178
Izod Impact, Notched 800 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
 70.0 kJ/m²
@Temperature 23.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Instrumented Impact Energy at Peak 65.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
 >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D 150
 3.0
@Frequency 1e+6 Hz
ASTM D 150
 3.0
@Frequency 60 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm
@Thickness 1.60 mm
ASTM D 149
 27.0 kV/mm
@Thickness 1.60 mm
IEC 60243-1
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D 150
 0.0010
@Frequency 60 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E 831
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KASTM C 177
 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 138 °C
@Thickness 3.20 mm
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
ASTM D 648
Vicat Softening Point 143 °CRate B/50; ASTM D 1525
 143 °CRate B/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D 542
 1.586ISO 489
Haze <= 0.80 %
@Thickness 2.54 mm
ASTM D 1003
Transmission, Visible 88 - 90 %
@Thickness 2.54 mm
ASTM D 1003
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPassesIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABIC2882 / 116770

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.