MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek SN102 Sinter-HIP Silicon Nitride
Categories: Ceramic; Carbide

Material Notes:

Information provided by CoorsTek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.23 g/cc0.117 lb/in³
Permeability 0.000.00Gas
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 290 GPa42100 ksi
Flexural Strength 1000 MPa145000 psi
Compressive Strength 3500 MPa508000 psi
Poissons Ratio 0.270.27
Fracture Toughness 6.00 MPa-m½5.46 ksi-in½KIC
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+16 ohm-cm<= 1.00e+16 ohm-cm
Dielectric Constant 8.158.15
Dielectric Strength 8.60 kV/mm
@Thickness 6.35 mm
218 kV/in
@Thickness 0.250 in
Dissipation Factor 0.00170.0017
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.50 µm/m-°C
@Temperature 25.0 - 1000 °C
1.94 µin/in-°F
@Temperature 77.0 - 1830 °F
Specific Heat Capacity 0.740 J/g-°C0.177 BTU/lb-°F
Thermal Conductivity 18.0 W/m-K125 BTU-in/hr-ft²-°FASTM-C408
Maximum Service Temperature, Air 1000 °C1830 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCOOR816 / 254564

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.