MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound 9X02785 Polycarbonate + PBT (PC+PBT) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: LNP STAT-KON 9X02785 compound is based on Polycarbonate / Polybutylene Terephthalate (PC/PBT) blend containing proprietary fillers. Added features of this grade include: Electrically Conductive.

Features: Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 64.0 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 2870 MPa50 mm/min; ASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 2890 MPaASTM D790
Izod Impact Notched 63.0 JASTM D256
Izod Impact, Unnotched 2160 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 - 1.00e+7 ohm-cmASTM D257
Surface Resistance 100 - 1.00e+7 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 280 °C
Middle Barrel Temperature 260 - 300 °C
Front Barrel Temperature 260 - 300 °C
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Roll Temperature 80.0 - 100 °C
Drying Temperature 120 °CInjection Molding
 120 °CFilm Extrusion
Dry Time 4.00 hourInjection Molding
 4.00 hourFilm Extrusion
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81164 / 289111

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.