MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials TSE3941M Silicone adhesive sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: TSE3941M is a one-component, fast curing silicone adhesive sealant that cures on exposure to atmospheric moisture to form an elastic silicone rubber. It has excellent corrosion-free adhesion to metals, including copper, plastics, ceramics, glass, etc. without the use of primers.

Features: Non-corrosive to metals; meets MIL-A-46146B corrosion test. Fast cure. Low odor cure; releases an alcohol vapor during cure. Primerless adhesion to many substrates. Excellent high and low temperature resistance: from -55 ºC to 200 ºC. Excellent weather ability, ozone, and chemical resistance. Excellent electrical insulation properties. Simple and easy-to-use one-component system.

Applications: Sealing of electrical and industrial applications. Connection sealing on electronic parts assemblies. Waterproof sealant for electrical, electronic and communication equipment.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccCured
Viscosity 50000 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63
Tensile Strength 3.20 MPa
Elongation at Break 70 %
Adhesive Bond Strength 1.40 MPaAluminum lap shear.
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+14 ohm-cmCured
Dielectric Constant 4.0
@Frequency 60 Hz
Cured
Dielectric Strength 21.0 kV/mmCured
Dissipation Factor 0.040
@Frequency 60 Hz
Cured
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.830 W/m-KCured
 
Processing PropertiesOriginal ValueComments
Processing Temperature 23.0 °C
@Time 605000 sec
Cure as Tested at 50% RH
Tack-Free Time 5.00 min
 
Descriptive Properties
AppearanceElastic rubberCured
 Flowable pasteUncured
ColorWhiteCured
 WhiteUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9974 / 265789

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.