MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones SCS1700 One-component, acetoxy cure silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: SCS1700 silicone sealant is a one-component, acetoxy cure silicone containing a fungicide that is supplied as a paste and upon cure, produces a durable, formed-in-place silicone rubber seal that is mildew and mold resistant. SCS1700 is an excellent candidate to consider the prevention of mildew formation around fixtures in areas such as locker rooms, swimming pool facilities and lavatories.

Features: Silicone Durability, Mildew Resistant, ±25% Movement Capacity. Application: SCS1700 is a candidate to consider: For use as a seal around bathtubs, shower stalls, wall fixtures, sinks, and other bathroom fixtures including countertops, soap fixtures, air dryers and drains. For grouting and bedding some ceramic tiles. In interior and exterior applications where areas are prone to mold and mildew formation.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 20 g/lUncured; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ASTM D2240
Tensile Strength, Ultimate 2.00 MPaASTM D412
Elongation, Ultimate 373 %ASTM D412
Peel Strength 30.4 pli
@Temperature 23.9 °C,
Time 1.81e+6 sec
50%RH; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air 55.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 122 °FApplication Temperature
Cure Time 48.0 - 72.0 hour
@Temperature 24.0 °C
1/4" deep section. 50% RH
Tack-Free Time 30.0 - 45.0 minASTM C679
Working Life 5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
ColorAlmondSCS1705
 TranslucentSCS1701
 WhiteSCS1702
Consistency / Sag0.1"
Joint Movement Capability±25%ASTM C719.
Silicone Content (%)100Uncured
UV & Weathering ResistanceExcellentGE 20 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9932 / 265743

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.