Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with <10% orientation. Information provided by Bayer Corporation, Plastics Division As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation. |