Eastman Cristal™ copolyester AN001 Natural has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but Eastman Cristal™ copolyester AN001 Natural maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. It is one of our premier materials for the cosmetics and personal care packaging market. Applications - Bottles-color cosmetics pkg
- Closures-fragrance pkg
- Color cosmetics packaging
- Fragrance packaging
- Personal care & cosmetics packaging
Key Attributes- Easy to extrude, cut, print, and seal
- Effective barrier properties
- Excellent chemical resistance
- Excellent clarity
- Excellent colorability
- Good impact strength
- Good stiffness
- High gloss appearance
- Toughness
Information provided by Eastman. |