MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DowAksa CarbonBond™ 200P Adhesive Putty System
Categories: Polymer; Thermoset; Epoxy

Material Notes: CarbonBond™ 200P is a high strength, toughened, structural epoxy adhesive for bonding of composite fabrics to substrate. CarbonBond™ 200P is a two phase (toughened) epoxy resin produced using a CTBN elastomer and a flexible resin backbone for maximum stress and fatigue resistance. CarbonBond™ 200P bonds with an immediate high tack consistency, a long working life and a quick cure time. The hardener provides >2 hour working life with full cures occurring between 6 hours to 7 days, depending on the cure temperature. It is recommended that the minimum application temperature should be at least 3°C above the dew point temperature. Unlike most epoxy adhesives, CarbonBond™ 200P adhesive cured at ambient temperatures provides heat resistance well in excess of most engineering limits (HDT of 180º F).

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.65 - 8.75 lb/galPart B
 9.70 - 9.80 lb/galPart A
pH 7.75Part A
 10.65 - 11Part B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Strength 4.50 ksiASTM D638
Elongation at Break 2.15 %ASTM D638
Tensile Modulus 344 ksiASTM D638
Flexural Strength 12.2 ksiASTM D790
Flexural Modulus 410.7 ksiASTM D790
Compressive Strength 11.3 ksiASTM D695
Compressive Modulus 571 ksiASTM D695
Adhesive Bond Strength 440 psito concrete
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °FHDT load not reported
Glass Transition Temp, Tg 75.0 °FASTM E1640
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 8.00 hourInitial
Pot Life >= 240 min1000g working life
 
Descriptive Properties
ColorBluePart B
 YellowPart A
Mix Ratio100:44 A:BWeight
 2:1 A:BVolume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWAK988 / 287935

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.