MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Protective Coating PC-Pool™ Epoxy
Categories: Polymer; Adhesive

Material Notes: Hand moldable epoxy putty that is especially designed for emergency type repairs where time is of the essence. The putty contains no solvents or VOCs. It is nonflammable and releases no noxious fumes. It doeso not shrink or pull away from surface. It is resistant to water, chemicals, and temperature extremes.

Putty is a hand mixed, fast-setting, epoxy putty for quick, permanent repairs to ceramics, glass, metals, concrete, wood, and numerous plastics. After 60 minutes the application can be sawed, sanded, tapped, drilled, machined, filled, and painted. The consistency eliminates drips and runs, promotes adhesion to the surface, and allows the material to be shaped and formed as needed before curing begins. PC-Pool Putty Epoxy™ cures to an off-white color. Suitable for interior or exterior applications.

Data provided by Protective Coating Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Compressive Yield Strength 55.2 MPa8000 psi
Adhesive Bond Strength 6.21 MPa900 psiTensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 3.00e+10 ohm3.00e+10 ohm
Dielectric Strength 11.8 kV/mm300 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Shrinkage <= 1.0 %<= 1.0 %
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 24.0 °C
1.00 hour
@Temperature 75.2 °F
Working Life 3.00 min
@Temperature 21.1 °C
3.00 min
@Temperature 70.0 °F
 
Descriptive Properties
ColorOff WhiteCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPXP97 / 280634

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.