MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SABIC SABIC® PP MB7450 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound MB7450 is a mineral filled modified polypropylene. The intended use of this material is in molding it in 1 to 1 ratio with SABIC® PP 90910 and as such not designed for sole use in applications. Using the material in the intended way will result in a molded part with a material with a property profile like SABIC® PPcompound 7450. SABIC® PPcompound MB7450 is a designated automotive grade. IMDS ID: 78695235

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³Injection molded sample ISO527-1A; ISO 1183
Filler Content 25 %25 %SABIC method
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength at Break 18.0 MPa2610 psiISO 527/1A
Tensile Strength, Yield 18.0 MPa2610 psiISO 527/1A
Elongation at Break 300 %300 %ISO 527/1A
Tensile Modulus 1.25 GPa181 ksiISO 527/1A
Flexural Modulus 1.30 GPa189 ksiISO 178/1A
Izod Impact, Notched (ISO) NBNBISO 180/1A
 10.0 kJ/m²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
N.B.: No Break; ISO 180/1A
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180/1A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11541 / 245008

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.