MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Celanex® DEV 3309 HRLT PBT, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Product Description: Celanex DEV 3309 HRLT is a 30% glass reinforced grade. It offers excellent physical properties, good laser transparency and hydrolysis resistance for laser welding applications.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Additive: Hydrolysis Resistant

Features: Hydrolysis Resistant

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccISO 1183
Water Absorption 0.16 %Equilibrium, 50% RH; ISO 62
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cmISO 294-4
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 21000 psiISO 527-2/5
Elongation at Break 2.3 %ISO 527-2/5
Tensile Modulus 1.52e+6 psiISO 527-1
Flexural Strength 33400 psiISO 178
Flexural Modulus 1.46e+6 psiISO 178
Charpy Impact, Notched 4.80 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 437 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 437 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 401 °FUnannealed; ISO 75-2/A
Vicat Softening Point 428 °FISO 306/B50
Glass Transition Temp, Tg 140 °FISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 482 - 500 °FHot Runner
Feed Temperature 446 - 464 °FInjection
Rear Barrel Temperature 446 - 464 °F
Middle Barrel Temperature 455 - 482 °F
Front Barrel Temperature 455 - 482 °F
Nozzle Temperature 482 - 500 °F
Zone 4 464 - 500 °FInjection
Melt Temperature 455 - 500 °F
Mold Temperature 149 - 248 °F
Drying Temperature 176 - 248 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6205 / 310898

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.