MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemours Teflon™ AF 2400 Amorphous Fluoroplastic Resins
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Teflon™ AF is a family of amorphous fluoroplastics similar to other amorphous polymers in optical clarity and mechanical properties, including strength. They also resemble fluoroplastics in their performance over a wide range of temperatures, outstanding electrical properties, and chemical resistance. They are distinct from other fluoroplastics in that they are soluble in selected solvents and have high gas permeability, high compressibility, high creep resistance, and low thermal conductivity. They have the lowest dielectric constant and refractive index of any known fluoroplastic. Products labeled AF 2400 and AF 2400 X are equivalent. Applications: optoelectronic devices, low-refractive index coating or covering for optical devices.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.67 g/cc1.67 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %
Permeability 490490N2. Barrer
 990990O2. Barrer
 28002800CO2. Barrer.
 40264026H2O. Barrer
Melt Flow 9.0 - 17 g/10 min
@Load 5.00 kg,
Temperature 260 °C
9.0 - 17 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  65
@Temperature 220 °C
65
@Temperature 428 °F
ASTM D1706
 75
@Temperature 23.0 °C
75
@Temperature 73.4 °F
ASTM D1706
Tensile Strength  2.40 - 6.00 MPa
@Temperature 220 °C
348 - 870 psi
@Temperature 428 °F
ASTM D638
 24.5 - 28.3 MPa
@Temperature 23.0 °C
3550 - 4100 psi
@Temperature 73.4 °F
ASTM D638
Tensile Strength, Yield  4.70 - 12.7 MPa
@Temperature 220 °C
682 - 1840 psi
@Temperature 428 °F
 24.5 - 28.3 MPa
@Temperature 23.0 °C
3550 - 4100 psi
@Temperature 73.4 °F
Elongation at Break  5.6 - 10.2 %
@Temperature 23.0 °C
5.6 - 10.2 %
@Temperature 73.4 °F
ASTM D638
 4.3 - 12.5 %
@Temperature 220 °C
4.3 - 12.5 %
@Temperature 428 °F
ASTM D638
Tensile Modulus 1.50 GPa218 ksiASTM D638
Flexural Modulus  0.600 - 0.800 GPa
@Temperature 220 °C
87.0 - 116 ksi
@Temperature 428 °F
ASTM D790
 1.50 - 1.70 GPa
@Temperature 23.0 °C
218 - 247 ksi
@Temperature 73.4 °F
ASTM D790
Taber Abrasion, mg/1000 Cycles 0.0500.050
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.91.9ASTM D150
Dielectric Strength 19.0 kV/mm483 kV/inASTM D149
Dissipation Factor 0.00010 - 0.000300.00010 - 0.00030ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FASTM D648
Glass Transition Temp, Tg 230 - 250 °C446 - 482 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.291.29ASTM D542
Abbe Number 113113
Transmission, Visible >= 95 %>= 95 %ASTM D1003
 
Descriptive Properties
Contact Angle with Water105ASTM D570
Critical Surface Energy15.6 Dynes/cm
Rockwell Hardness97.5ASTM D785. 23°C
Volume Coefficient of Thermal ExpansionASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8775 / 268701

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.