MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PE-HD Hard PE, low-pressure PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HD-PE is more rigid and abrasion-resistant than soft PE. It is characterized by its resistance to low temperatures of up to –50 °C and high temperatures of max. +80 °C.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccDIN EN ISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64DIN EN ISO 868
Ball Indentation Hardness 40.0 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 22.0 MPa50 mm/min; DIN EN ISO 527
Elongation at Yield 9.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 0.900 GPa1 mm/min; DIN EN ISO 527
Charpy Impact Unnotched NBDIN EN ISO 179-1eU
Charpy Impact, Notched 19.0 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Strength 47.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µm/m-°CDIN 53752
Thermal Conductivity 0.380 W/m-K
Maximum Service Temperature, Air 80.0 °Clong term
Minimum Service Temperature, Air -50.0 °C
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP003 / 250501

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.