MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Valley Adhesives EM-422 High Temperature Application Glue Stick
Categories: Polymer; Adhesive; Thermoset

Material Notes: Valley Adhesives EM-422 High Temperature Application Glue Stick
Rapid strength build up; Excellent hot tacking and wetting; Bonds corrugated boxes and paper in packaging operations and repackaging areas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2162 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88
Tensile Strength, Ultimate 641 psi
Elongation at Break 198 %
Shear Strength 563 psi
Peel Strength 23.7 pli
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °FHeat Resistance Value at 2 psi.
Softening Point 208 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.80 secHot tack
Pot Life 25 secOpen Time
 
Descriptive Properties
ColorOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Bostik 6332 Quick Setup EVA Glue Stick
Bostik 2385 General Purpose EVA Glue Stick
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick

PVALL07 / 71811

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.