MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound DE002ER Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DE002ER compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Easy Molding. Mold Release, Electrically Conductive.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Good Mold Release,Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.170 %0.170 %23°C/50% RH/24 hrs; ASTM D570
 0.660 %0.660 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00060 - 0.0032 cm/cm0.00060 - 0.0032 in/in24hrs; ISO 294
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in24hrs; ASTM D955
 0.0029 - 0.0043 cm/cm0.0029 - 0.0043 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiASTM D638
 102 MPa14800 psiISO 527
Elongation at Break 2.8 %2.8 %ASTM D638
 3.3 %3.3 %ISO 527
Tensile Modulus 6.80 GPa986 ksi1 mm/min; ISO 527
 6.96 GPa1010 ksi50 mm/min; ASTM D638
Flexural Strength 165 MPa23900 psiASTM D790
 170 MPa24700 psiISO 178
Flexural Modulus 6.13 GPa889 ksiASTM D790
 6.96 GPa1010 ksiISO 178
Izod Impact Notched 95.0 J70.1 ft-lbASTM D256
Izod Impact, Unnotched 5.63 J/cm10.5 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 39.0 kJ/m²18.6 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 19.0 J14.0 ft-lbpeak; ASTM D3763
Impact Test 4.00 J2.95 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  26.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 26.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  58.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
32.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 58.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
32.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
@Thickness 3.20 mm
289 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °C288 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 141 °C
@Thickness 3.20 mm
286 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.60 mm
V-1
@Thickness >=0.0630 in
UL 94
 V-0
@Thickness >=3.40 mm
V-0
@Thickness >=0.134 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81206 / 289153

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.