MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron® FST PA66 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Nylatron® FST Polyamide PA66 shapes are fire, smoke, and toxicity retardant, which enables them to withstand high temperatures. In addition to these characteristics, Nylatron® FST PA66 is also JAR / FAR 25.853 compliant. As the first engineering plastic to achieve this standard, this grade was also developed specifically for aircraft interior environments, and is often favored as a replacement for metal parts applications, such as brackets, seal bushings, slide rails, and duct seals.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccISO 1183-1
Water Absorption 0.53 %
@Time 86400 sec
immersion in water; ASTM D570
Water Absorption at Saturation 7.4 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88ISO 2039-2
Tensile Strength 90.0 MPaISO 527-1/-2
Elongation at Break 1.5 %ISO 527-1/-2
Elongation at Yield 7.0 %ISO 527-1/-2
Modulus of Elasticity 3.50 GPaISO 527-1/-2
Compressive Strength 30.0 MPa
@Strain 1 %
ISO 604
 60.0 MPa
@Strain 2 %
ISO 604
 99.0 MPa
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 4.90 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Surface Resistivity per Square 1.00e+12 ohmANSI/ESD STM 11.11
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 686 V/milIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
Melting Point 260 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CISO 75-1/-2
Minimum Service Temperature, Air -30.0 °C
Flammability, UL94 V-2
@Thickness 3.00 mm
Oxygen Index 26 %ISO 4589-1/-2
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM910 / 291067

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.