MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Synthos CAM24 CAM impact modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAM is a new PVC impact modifier, which is an interpenetrating network copolymer formed by grafting slightly chlorinated HDPE with acrylate. Its main function is to enhance the impact strength of PVC finished products under low temperature and endows the better toughness and impact modifier in low temperature. At same time, it can improve the weather ability of products. CAM is mainly used in PVC pipes, fittings and injections

Performance:

  • Excellent elongation rate at break and toughness
  • Excellent impact strength under low temperature
  • High cost-effective
  • Better weather-resistance
  • Better surface glossiness for PVC finished products
Application: Mainly used to produce opaque PVC products, such as PVC profiles, PVC pipes, PVC siding etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.600 g/ccGB/T 1636-2008
Volatiles <= 1.5 %ASTM D5668
Particle Mesh Size 30 Mesh<2%; GB/T2916
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 6.00 MPaGB/T 528-2009
Elongation at Break 1200 - 1400 %GB/T 528-2009
 
Descriptive Properties
AppearanceWhite Power

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW210 / 320241

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.