MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shanghai Potomer CR2442 Polychloroprene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CR244 is a special chloroprene rubber of high-crystallization rate made by polymerizing the emulsion with nonsulfur modifier as modifying agent and with Lomar Pw as disperser, and similar to Japanese polychloroprene rubber Type A--90.

Characteristics: CR244 is characterized by high crystallization rate , strong cohesion, comparatively high adhesion strength and excellent ozone resistance, weather resistance, oil resistance and combustion retardancy.

Appearance: Milky white to light brown lumpy matter free from mechanical impurities except talc power.

Application: CR244 is a basic raw material for adhesive production, and its preparation can be applied to adhesion for rubber , leather, timber and metal.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.3 %
Brookfield Viscosity 3000 - 7000 cP15% toluene solution (mPa.s at 25 + 0 . 1) ºC
Mooney Viscosity 44 - 52
@Temperature 100 °C
MS 2+2.5
Ash <= 1.3 %
 
Mechanical PropertiesOriginal ValueComments
Peel Strength >= 75.0 kN/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM056 / 284502

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.