Hostacom PT975X PC81 is a 12% talc filled PP copolymer, with high melt flow rate and high stiffness. Product is available as a customized color matched, pellet form. This grade is delivered in PC81 color version. Applications: Interior TrimsInformation provided by LyondellBasell. |