EXTEM AMHH811F filament is a thermoplastic polyimide (TPI) product for additive manufacturing applications with a glass transition temperature (Tg) of 247 °C. The filament provides high heat resistance and halogen free, thin wall FR capability with a UL94 V-0 listing at 0.75 mm (Blue Cards are available on the UL IQ Database). Information provided by SABIC |