MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PSU High-performance plastic
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: These PSU semi-finished products are manufactured from a non-UV-stabilized polysulfone raw material. This material offers very good resistance to radiation, good ionic purity, and favourable resistance to chemicals and hydrolysis. In comparison with PEI, PSU has a lower profile of properties and is often used as a replacement for polycarbonate if higher temperature resistance, improved chemical resistance, and steam sterilization options are required. PSU is often used in the food processing industry (for milking machines, pumps, valves, filter plates, and heat exchangers) and for technical medical components which need to be repeatedly cleaned and sterilized.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccDIN EN ISO 1183-1
Water Absorption 0.060 %
@Time 86400 sec
DIN EN ISO 62
Moisture Absorption 0.200 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85DIN EN ISO 868
Ball Indentation Hardness 155 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 80.0 MPaDIN EN ISO 527
Elongation at Break 15 %DIN EN ISO 527
Modulus of Elasticity 2.60 GPaDIN EN ISO 527
Charpy Impact, Notched 6.00 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 50 Hz
IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243
Dielectric Loss Index 0.0010
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 125 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 0.260 W/m-K
Maximum Service Temperature, Air 160 °Clong term
 180 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 175 °CDIN EN ISO 75 / A
Minimum Service Temperature, Air -50.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 V-0
@Thickness 6.00 mm
 
Descriptive Properties
Colornatural (yellow, transparent)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP052 / 250550

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.