MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Ultimaker Tough PLA Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description: Ultimaker Tough PLA is a technical PLA filament with toughness comparable to Ultimaker ABS. Ideal for reliably printing technical models at large sizes, our Tough PLA offers the same safe and easy use as regular PLA

Key features: With an impact strength similar and higher stiffness compared to Ultimaker ABS, Tough PLA is less brittle than regular PLA and gives a more matte surface finish quality. Heat resistance is similar to standard PLA filaments, so printed parts should not be exposed to temperatures above 60 °C

Applications: Functional prototyping, tooling, manufacturing aids

Non-suitable for: Food contact and in vivo applications. Long term outdoor usage or applications where the printed part is exposed to temperatures higher than 60 °C

Information provided by Ultimaker

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Filament Diameter 2750 - 2950 µm
Melt Flow 6.0 - 7.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79
Tensile Strength at Break 37.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 37.0 MPa50 mm/min; ISO 527
Elongation at Break 3.1 %50 mm/min; ISO 527
Elongation at Yield 3.1 %50 mm/min; ISO 527
Tensile Modulus 1820 MPa1 mm/min; ISO 527
Flexural Strength 78.0 MPaISO 178
Flexural Modulus 2490 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.62
@Frequency 1e+6 Hz
ASTM D150-11
Dissipation Factor 0.014
@Frequency 1e+6 Hz
ASTM D150-11
 
Thermal PropertiesOriginal ValueComments
Melting Point 151 °C
Vicat Softening Point 63.0 °CISO 306
Glass Transition Temp, Tg 62.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PULTIMK001 / 281740

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.