MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Accelerator THIO #1
Categories: Other Engineering Material

Material Notes: Product Description: Accelerator Thio #1 is a non-discoloring accelerator for use in Neoprene (CR), Natural Rubber, EPDM and many other elastomers. Thio #1 provides rapid acceleration and can be used in latex and cement applications.

Application: Thio #1 is a very effective Neoprene (CR) rubber accelerator providing fast, safe cures with flat curing plateaus (no marching modulus). It also functions as an accelerator for compounds based on Neoprene (CR) latex, Natural Rubber latex and cements. Thio #1 activates thiazole accelerators and can be used in light colored compounds since it is essentially non-discoloring. It can also be used in EPDM sponge applications. In Neoprene, typical dosages range from 0.5 to 1.5 phr for carbon black and mineral loaded compounds. Recommended Neoprene (CR) latex dosages start at 0.5 phr. In extruded EPDM closed cell sponge application Thio #1 can be used at a level of 1.5 to 3.0 phr. Thio #1 is approved for use in rubber in repeated contact with foodstuffs under CFR 21, Regulation 177.2600, Accelerators (1,3-Diphenyl-2-thiourea) not to exceed 1.5% by weight.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Particle Mesh Size 100 Mesh0.001
Ash 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 148 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.70 %
 
Descriptive Properties
AppearanceOff-white powder
Purity0.98

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH454 / 315372

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.