Eastman TREVA™ TR6011 Natural is a cellulose-based engineering bioplastic that offers both high performance and enables exceptional depth of color and high gloss for opaque applications. TREVA™ is chemically resistant, dimensionally stable and has excellent flow, BPA-free and enables exceptional depth of color and high gloss for opaque applications. The United States Department of Agriculture’s (USDA’s) BioPreferred® program has Certified Eastman TREVA™ Engineering Bioplastic TR6011 with a biobased content of 45%. Key Attributes - BPA-free
- Dimensional stability
- Excellent chemical resistance
- Excellent flow
- Good clarity
- Low birefringence
Information provided by Eastman. |