MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI THERMODAN® HF 0103-212 NT Non-halogen flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: SACO AEI Polymers THERMODAN® HF 0103-212NT is a flame retardant non-halogen thermoplastic wire and cable compound. It is designed for use in a variety of jacketing applications. This compound has superior fire performance including slow flame propagation, low smoke production and low smoke corrosivity. It can be used as a jacket compound on cables recognized under UL 1277 tray cables and can pass flame retardant requirements set forth under UL 1685, IEEE 1202 and FT-4. THERMODAN® HF 0103-212NT is recognized under UL 2885 as being halogen free. It is natural in color and UV resistant.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
pH 6.7of Gases; IEC 60754-2
Melt Flow 4.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 4.44 - 26.7 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94
@Time 1.00 sec
ASTM D2240
Hardness, Shore D 55
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1800 psiASTM D638
 1570 psi
@Time 2.59e+6 sec
Weather-o-meter; ASTM D638
 1710 psi
@Treatment Temp. 100 °C,
Time 346000 sec
Oil; ASTM D638
 2250 psi
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
Elongation at Break 215 %ASTM D638
 187 %
@Time 2.59e+6 sec
Weather-o-meter; ASTM D638
 155 %
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
 204 %
@Treatment Temp. 100 °C,
Time 346000 sec
Oil; ASTM D638
Flexural Modulus 12900 psi1% secant; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °CISO 4589-3
Brittleness Temperature -19.0 °CASTM D746
Smoke Density <= 150Flaming, Dsmax (corrected); ASTM E662-13a
 <= 250Non-flaming, Dsmax (corrected); ASTM E662-13a
 <= 30
@Time 240 sec
Non-flaming, Ds; ASTM E662-13a
 <= 35
@Time 240 sec
Flaming, Ds; ASTM E662-13a
Oxygen Index 38 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 300 - 320 °F
Zone 2 330 - 350 °F
Zone 3 350 - 370 °F
Zone 4 350 - 370 °F
Die Temperature 370 - 390 °F
Melt Temperature 360 - 380 °F
Head Temperature 340 - 360 °F
 
Descriptive Properties
Acid Gas<5 mg/gIEC 60754-1
Conductivity of Gases0.51 µS/mmIEC 60754-2 (Fire/Smoke)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO079 / 265509

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.