MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BRP Manufacturing CH711 Epichlorohydrin Rubber Sheet
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material: Epichlorohydrin Rubber Sheet
BRP Style: CH711 – Style 4820 – H523
Finish: Smooth or Nylon
ASTM Callout: ASTM D2000 M2CH705A25B34EF31EO15EO35F17

Information provided by BRP Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1200 psiOriginal; ASTM D412
 <= 900 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged; ASTM D573
 840 - 1560 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged; ASTM D865
Elongation at Break 200 %Original; ASTM D412
 <= 100 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged; ASTM D865
 <= 100 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged; ASTM D573
Compression Set <= 25 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395 Method B
 <= 50 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -40.0 °F
 
Descriptive Properties
Hardness55-85Heat Aged, ASTM D865, 70 h @ 125°C
 60-85A25 - Heat Resistance, ASTM D573, 70 hours @ 125°C
 65-75ASTM D2240
Oil Immersion<30% Volume ChangeASTM D471, IRM 903 Oil, 70 h @ 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRPM062 / 315723

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.