MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem PA-80 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Description: PA-80 Rubber is a pre-crosslinked natural rubber which acts a processing aid when blended with natural rubber, SBR, neoprene or nitrile rubber.

Recommended Uses:
Extrusions: Compounds containing PA-80 Rubber maintain extruded shape, extrude faster, smoother and with less die swell. Nerve of the compound is reduced significantly allowing closer extrusion tolerances.
Calendering: Compounds containing PA-80 Rubber give smoother sheets with closer tolerances.
Open Steam Cures: Compounds containing PA-80 Rubber have less tendency to deform during open steam cure because of the presence of the crosslinked polymer.

Composition: PA-80 Rubber is produced from a mixture of 80% pre-cured latex and 20% uncured latex which is coagulated and processed by conventional plantation methods to give a pale crepe grade natural rubber in compressed crumb form.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Content0.16Accelerator EZ
 0.32MBT
 1.2Zinc Oxide
 1.6Sulfur
 100Natural Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH180 / 315098

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.