MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Cabot CABELEC® CA3178 Nylon 6, Conductive Compound
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product highlights: CABELEC CA3178 electrically conductive compound is made from a conductive carbon black dispersed in polyamide 6. Its electrical and mechanical properties are not impacted by normal atmospheric conditions. It is suitable for use in injection molding applications.

Key applications: CABELEC CA3178 conductive compound is suitable for use in products for packaging and handling of electronic products where it is desirable to mitigate the hazard of electrostatic discharge.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.196 g/cc0.04321 lb/in³ISO 1183
Linear Mold Shrinkage 0.015 - 0.020 cm/cm0.015 - 0.020 in/inASTM D955
Melt Flow 10 g/10 min
@Load 275 kg,
Temperature 10.0 °C
10 g/10 min
@Load 606 lb,
Temperature 50.0 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 78
@Time 15.0 sec
78
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 45.0 MPa6530 psiISO 527
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break 15 %15 %ISO 527
Flexural Strength 89.0 MPa12900 psiISO 178
Flexural Modulus 2.70 GPa392 ksiISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180A
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 61340-2-3
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 61340-2-3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FISO 75
Vicat Softening Point 215 °C
@Load 1.02 kg
419 °F
@Load 2.25 lb
ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 °C428 °Fbarrel
Nozzle Temperature 275 °C527 °F
Mold Temperature 60.0 °C140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT040 / 315775

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.