MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman 812A Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.

Unless otherwise noted, all tests are run at 23°C and 50% RH.

Information from manufacturer data sheet.

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Key Words: Specialty injection molding applications in the medical market
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.909 g/cc0.0328 lb/in³ASTM D4883
Melt Flow 200 g/10 min
@Load 2.16 kg,
Temperature 190 °C
200 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 6.00 MPa870 psi500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Tensile Strength, Yield 8.00 MPa1160 psi500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Elongation at Break 100 %100 %500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Flexural Modulus 0.103 GPa
@Strain 2 %
14.9 ksi
@Strain 2 %
Secant; 12.7 mm/min. (0.5 in./min.); ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 67.0 °C153 °FASTM D1525
Brittleness Temperature -28.0 °C-18.4 °FASTM D746
 
Descriptive Properties
ProcessInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications
Westlake Plastics Lennite® GUR1020 (Type I) UHMW-PE For Medical Applications
Eastman 812P Polyethylene
Versalis Riblene® MY 00 Low Density Polyethylene - Injection Molding

PEAT330 / 35376

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.