MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX674PC Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 674PC resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less powder coat painting around corners and holes with a Class A Surface. NORYL GTX674PC resin exhibits high heat resistance, improved surface appearance and is an excellent candidate for automotive applications such as mirror housings and brackets. This material is only available in black.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Heat Stabilized,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Moisture Absorption 0.0700 %Injection Molding
Linear Mold Shrinkage, Flow 0.010 - 0.013 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 64.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ASTM D638
Elongation at Break 4.0 %50 mm/min; ASTM D638
 4.0 %50 mm/min; ISO 527
Elongation at Yield 3.0 %50 mm/min; ASTM D638
 3.0 %50 mm/min; ISO 527
Tensile Modulus 2810 MPa5 mm/min; ASTM D638
Flexural Strength 103 MPayield, 2 mm/min; ISO 178
 109 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2480 MPa2 mm/min; ISO 178
 2890 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 74.0 JASTM D256
 50.0 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 4.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 - 10000 ohm-cmSABIC method
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 0.750 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 81.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 86.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 185 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 188 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 196 °CRate B/120; ISO 306
 197 °CRate B/50; ASTM D1525
 197 °CRate B/50; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 305 °C
Zone 2 270 - 305 °C
Zone 3 275 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82127 / 290074

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.