MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 323 Two component, addition cured silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Convenient handling
  • Optically clear in thin sections
  • Low to moderate viscosity
  • Excellent strength properties
Product Description: Master Bond MasterSil 323 is a two component silicone for high performance bonding, sealing, and encapsulating. It does not require air when polymerizing and does not outgas while curing. It has a forgiving one to one mix ratio by weight. The viscosity of both Parts A and B allows for easy mixing and good flow. It is a low exothermic material with a long open time of about 2-3 hours. It cures at ambient temperatures in 48-72 hours or in 2-4 hours at 135- 165°F. The optimum cure is overnight at room temperature followed by 2-4 hours at 135-165°F. This silicone contains no solvents or diluents and has very low shrinkage upon curing. It has a Shore A hardness of 35 to 45. MasterSil 323 bonds well to a wide variety of substrates including metal, glass, plastics and ceramics, as well as to silicone rubber. It can withstand the most rigorous kinds of thermal shock and cycling without cracking or exerting stress on components. The service temperature range is from -65°F to +400°F. Other noteworthy features are its optical clarity, especially in thinner sections, and its superior electrical insulation profile. MasterSil 323 should be considered in optical, electronic, aerospace, and specialty OEM applications where a high strength, optically clear, easy to use, silicone is needed.

Product Advantages:

  • Addition cured, no by-products released during cure
  • Flowable, with long open time
  • Optically clear, especially in thin sections
  • Good bond strength, yet potentially removable
  • Low dielectric constant

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 10000 - 25000 cPPart B
 15000 - 30000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35 - 45
Tensile Strength 100 - 200 psi
Elongation at Break 150 - 250 %
Tensile Modulus 100 - 175 psi
Adhesive Bond Strength 200 - 250 psiTensile lap shear, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 2.8
@Frequency 1e+6 Hz
Dielectric Strength 450 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 400 - 450 µm/m-°C
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -65.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.44
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Temperature 57.2 - 73.9 °C
Optimum: Overnight at 75°F followed by 2-4 hours at 135-165°F
 2.00 - 4.00 hour
@Temperature 57.2 - 73.9 °C
Option 2
 48.0 - 72.0 hour
@Temperature 23.9 °C
Option 1
Working Life 2.00 - 3.00 hourafter mixing, 100 gram batch
Shelf Life 6.00 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio1:1 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5935 / 306824

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.