MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC ULTEM™ Resin CRS5001 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing.

Features: High Stiffness,Hydrolytic Stability,Enhanced Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Transparent

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0600 %0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.2 %1.2 %ISO 62-1
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 360 °C
7.0 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 135 MPa19600 psiH358/30; ISO 2039-1
Tensile Strength at Break 95.0 MPa13800 psi50 mm/min; ISO 527
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527
Elongation at Break 50 %50 %50 mm/min; ISO 527
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527
Tensile Modulus 3.20 GPa464 ksi1 mm/min; ISO 527
Flexural Strength 105 MPa15200 psibreak, 2mm/min; ISO 178
 110 MPa16000 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 50.0 - 60.0 Hz
3.2
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength  16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
660 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
Dissipation Factor  0.0016
@Frequency 50.0 - 60.0 Hz
0.0016
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0043
@Frequency 1e+6 Hz
0.0043
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Comparative Tracking Index 125 V125 VIEC 60112
 100 - 175 V100 - 175 VUL 746A
 175 V175 VIEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
>= 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
@Temperature -20.0 - 150 °C
30.0 µin/in-°F
@Temperature -4.00 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 57.0 µm/m-°C
@Temperature -20.0 - 150 °C
31.7 µin/in-°F
@Temperature -4.00 - 302 °F
ISO 11359-2
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 220 °C428 °FRate B/50; ISO 306
 222 °C432 °FRate B/120; ISO 306
 225 °C437 °FRate A/50; ISO 306
UL RTI, Electrical 160 °C320 °FUL 746B
UL RTI, Mechanical with Impact 160 °C320 °FUL 746B
UL RTI, Mechanical without Impact 160 °C320 °FUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
Oxygen Index 47 %47 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 360 - 400 °C680 - 752 °F
Zone 2 350 - 390 °C662 - 734 °F
Zone 3 370 - 410 °C698 - 770 °F
Melt Temperature 360 - 410 °C680 - 770 °FInjection Molding
Mold Temperature 120 - 170 °C248 - 338 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °C176 - 248 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82678 / 290625

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.