MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Hytrel® ECO 6356B TPC Polyester Elastomer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 63 Shore D High Performance Polyester Elastomer certified bio-circular according to ISCC Plus mass balance approach

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Melt Density 1.06 g/cc0.0383 lb/in³
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
Sim. to ISO 62
 0.60 %
@Thickness 2.00 mm
0.60 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4, 2577
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ISO 48-4 / ISO 868
 6363ISO 868
Tensile Strength, Yield  12.0 MPa
@Strain 5.0 %
1740 psi
@Strain 5.0 %
ISO 527-1/-2
 15.0 MPa
@Strain 10 %
2180 psi
@Strain 10 %
ISO 527-1/-2
Tensile Modulus 0.280 GPa40.6 ksiISO 527-1/-2
50% Modulus 18.8 MPa
@Strain 50 %
18.8 MPa
@Strain 50 %
ISO 527-1/-2
100% Modulus 19.0 MPa
@Strain 100 %
2760 psi
@Strain 100 %
ISO 527-1/-2
Flexural Modulus 0.290 GPa42.1 ksiISO 178
Poissons Ratio 0.480.48
Izod Impact, Notched (ISO)  19.0 kJ/m²
@Temperature -40.0 °C
9.04 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 81.0 kJ/m²
@Temperature 23.0 °C
38.5 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  1.50 J/cm²
@Temperature -40.0 °C
7.14 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
Tensile Impact Strength 300 kJ/m²
@Temperature 23.0 °C
143 ft-lb/in²
@Temperature 73.4 °F
Notched; ISO 8256/1
Tensile Creep Modulus, 1 hour 248 MPa36000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 182 MPa26400 psiISO 899-1
Tear Strength 145 kN/m827 plinormal; ISO 34-1
 158 kN/m902 pliparallel; ISO 34-1
Abrasion 110110mm³; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+11 ohm-cm8.00e+11 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 62631-3-2
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.6
@Frequency 100 Hz
4.6
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Dissipation Factor  0.012
@Frequency 100 Hz
0.012
@Frequency 100 Hz
IEC 62631-2-1
 0.036
@Frequency 1e+6 Hz
0.036
@Frequency 1e+6 Hz
IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 190 µm/m-°C106 µin/in-°FISO 11359-1/-2
 160 µm/m-°C
@Temperature -40.0 - 23.0 °C
88.9 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 190 µm/m-°C
@Temperature 23.0 - 55.0 °C
106 µin/in-°F
@Temperature 73.4 - 131 °F
ASTM E 831
CTE, linear, Transverse to Flow 176 µm/m-°C97.8 µin/in-°FISO 11359-1/-2
 150 µm/m-°C
@Temperature -40.0 - 23.0 °C
83.3 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 170 µm/m-°C
@Temperature 23.0 - 55.0 °C
94.4 µin/in-°F
@Temperature 73.4 - 131 °F
ASTM E 831
Specific Heat Capacity 2.15 J/g-°C0.514 BTU/lb-°FMelt
Thermal Conductivity 0.150 W/m-K1.04 BTU-in/hr-ft²-°FMelt; ISO 22007-2
Melting Point 210 °C410 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Vicat Softening Point 100 °C212 °F50°C/h, 50N; ISO 306
 195 °C383 °F50°C/h 10N; ISO 306
Brittleness Temperature -96.0 °C-141 °FISO 974
Glass Transition Temp, Tg -5.00 °C23.0 °F10°C/min; ISO 11357-1/-3
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
Oxygen Index 21 %21 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 °C446 °FOptimum
 225 - 240 °C437 - 464 °F
 240 °C464 °FOptimum
 235 - 260 °C455 - 500 °F
Mold Temperature 45.0 °C113 °FOptimum
 45.0 - 55.0 °C113 - 131 °F
Drying Temperature 100 °C212 °F
 90.0 - 110 °C194 - 230 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer
 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %
 <= 0.080 %<= 0.080 %
Hold Pressure <= 70.0 MPa<= 10200 psi
 
Descriptive Properties
AdditivesBiobased
Drying Recommended?yes
Eff. thermal diffusivity (m²/s)5.44E-08
Emission of organic compounds µgC/g2.5VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
Fogging0.1 mgG-value (condensate); ISO 6452
Odor Class2.5VDA 270
PolymerTPC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5195h / 295971

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.