MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin FE1630PW Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ FE1630PW resin is a 30% glass reinforced blend of polyphenylene ether (PPE) + crystal clear polystyrene (ccPS). This injection moldable material is FC EU, FDA food contact compliant, NSF/ANSI 61*ACS, WRAS, KTW, and W270 listed for global potable water use. NORYL FE1630PW resin exhibits excellent long-term hydrolytic stability, very low moisture absorption, heat / hot water resistance and is an excellent candidate for a variety of water management applications such as pump housings, impellers, shower/faucet, membrane housings and valves. *NSF certification is color dependent.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 30 cP
@Load 10.0 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 240 MPaH358/30; ISO 2039-1
Tensile Strength at Break 133 MPa5 mm/min; ISO 527
 134 MPa5 mm/min; ASTM D638
Elongation at Break 2.4 %5 mm/min; ASTM D638
 2.5 %5 mm/min; ISO 527
Tensile Modulus 9570 MPa5 mm/min; ASTM D638
 9600 MPa1 mm/min; ISO 527
Flexural Strength 192 MPabreak, 2mm/min; ISO 178
Flexural Modulus 7760 MPa1.3 mm/min, 50 mm span; ASTM D790
 8120 MPa2 mm/min; ISO 178
Izod Impact Notched 85.0 JASTM D256
 75.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 505 J/mASTM D4812
 465 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 30.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 30.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 65CS-17, 1 kg; SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 145 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 145 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 154 °CRate B/50; ISO 306
 158 °CRate B/120; ISO 306
 165 °CRate A/50; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 800 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 775 °C
@Thickness 3.00 mm
IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 320 °C
Zone 2 280 - 300 °C
Zone 3 300 - 310 °C
Melt Temperature 290 - 320 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82292 / 290239

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.