MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici Radiflam® A RV500 AF 821 BR Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: PA66 flame retardant, injection molding grade, with red phosphorus. 50% glass fiber reinforced. Natural red brick color.

Suitable for parts requiring fire retardancy along with high stiffness and mechanical resistance. Improved glow wire behavior. Typically employed for domestic appliances.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 240 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 2.8 %5 mm / min. DAM; ISO 527-2/1A
Tensile Modulus 17500 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 380 MPa2mm / min. DAM; ISO 178
Flexural Modulus 15600 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 16.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
Comparative Tracking Index 600 VDAM. Sol.A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/2Af
Flammability, UL94 V-0
@Thickness 0.800 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
IEC 60695-2-1/3
 775 °C
@Thickness 2.00 mm
IEC 60695-2-1/3
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-1/2
 960 °C
@Thickness 2.00 mm
IEC 60695-2-1/2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 100 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium-high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6984 / 293489

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.