MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EOS StainlessSteel PH1 DMSL on EOS M 290
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel

Material Notes: EOS StainlessSteel PH1 is a pre-alloyed stainless steel in fine powder form. The chemistry of EOS StainlessSteel PH1 conforms to the compositions of DIN 1.4540 and UNS S15500. This kind of steel is characterized by having good corrosion resistance and excellent mechanical properties, especially in the precipitation hardened state. This type of steel is widely used in variety of engineering applications requiring high hardness, strength and corrosion resistance. This material is ideal for many part-building applications (DirectPart) such as functional metal prototypes, small series products, individualized products or spare parts. Standard processing parameters use full melting of the entire geometry with 20 µm layer thickness. Using standard parameters the mechanical properties are fairly uniform in all directions. Parts made from EOS StainlessSteel PH1 can be machined, spark-eroded, welded, micro shot-peened, polished and coated if required.

Typical applications:

  • engineering applications including functional prototypes, small series products, individualized products or spare parts.
  • parts requiring high corrosion resistance, sterilizability, etc.
  • parts requiring particularly high hardness and strength.

Information provided by EOS GmbH (Electro Optical Systems).

Key Words: UNS S15500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/ccISO 3369
Particle Size <= 63 µm<0.5 wt% above 63µm; ASTM B214
Thickness 20.0 micronsLayer Thickness
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 40DIN EN ISO 6508-1
Tensile Strength, Ultimate 1150 - 1250 MPaAs built, horizontal direction (XY); ISO 6892:1998
 1150 - 1250 MPaAs built, vertical direction (Z); ISO 6892:1998
 1340 - 1540 MPa
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, vertical direction (Z); ISO 6892:1998
 1350 - 1550 MPa
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, horizontal direction (XY); ISO 6892:1998
Tensile Strength, Yield 855 - 1005 MPaAs built, vertical direction (Z); ISO 6892:1998
 940 - 1110 MPaAs built, horizontal direction (XY); ISO 6892:1998
 1200 - 1400 MPa
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, vertical direction (Z); ISO 6892:1998
 1250 - 1450 MPa
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, horizontal direction (XY); ISO 6892:1998
Elongation at Break 10 - 18 %As built, vertical direction (Z); ISO 6892:1998
 13 - 21 %As built, horizontal direction (XY); ISO 6892:1998
 10 - 16 %
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, vertical direction (Z); ISO 6892:1998
 12 - 18 %
@Treatment Temp. 525 °C,
Time 14400 sec
Heat treated, horizontal direction (XY); ISO 6892:1998
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 14 - 15.5 %
Copper, Cu 2.5 - 4.5 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.50 %
Nickel, Ni 3.5 - 5.5 %
Niobium, Nb (Columbium, Cb) 0.15 - 0.45 %
Silicon, Si <= 1.0 %
 
Descriptive Properties
Surface roughness< 0.5 µmRz, after polishing
 25.0 µmRz, after shot-peening
 5.0 µmRa, after shot-peening
Volume rate2.0 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NEOS950 / 280610

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.