MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ ATX3562R PEI (Europe)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 50% Glass Fiber

Material Notes: 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.69 g/ccASTM D792
Density 1.69 g/ccISO 1183
Moisture Absorption 0.0400 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.10 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 20 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 20 g/10 min
@Load 5.00 kg,
Temperature 360 °C
MVR, cm^3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 121 MPa5 mm/min; ISO 527
 125 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 121 MPa5 mm/min; ISO 527
 125 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 1.4 %5 mm/min; ISO 527
 2.5 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.4 %5 mm/min; ISO 527
 2.5 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 172 MPa2 mm/min; ISO 178
 180 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 12900 MPa1.3 mm/min, 50 mm span; ASTM D790
 13550 MPa2 mm/min; ISO 178
Izod Impact, Notched 50.0 J/mASTM D256
 49.0 J/m
@Temperature -30.0 °C
ASTM D256
 111 J/m
@Thickness 3.20 mm
Reverse Notched; ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1U
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 12.0 JASTM D3763
Tangent Modulus 14690 MPa1 mm/min; ISO 527
 14940 MPa5 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+15 ohm-cmASTM D257
Surface Resistance 2.10e+15 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
 16.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 38.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
 38.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 195 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 182 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 183 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 184 °CRate B/50; ASTM D1525
 187 °CRate B/50; ISO 306
 195 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 350 - 370 °C
Zone 1 340 - 360 °C
Zone 2 345 - 365 °C
Zone 3 350 - 370 °C
Melt Temperature 350 - 370 °C
Mold Temperature 135 - 165 °C
Drying Temperature 135 °C
Dry Time 4.00 - 6.00 hour
 10.0 hourCumulative
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
THERMALPassesIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI22734 / 215870

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.